Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kraton D1161 P - TPS - Kraton Polymers

Material Data Center offers the following functions for Kraton D1161 P:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kraton D datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Kraton D1161 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 13.5 g/10min ASTM D 1238
Température 200 °C -
Charge 5 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module à 300% allongement 0.896 MPa ASTM D 412
Dureté A Shore 32 - ASTM D 2240
Module de traction 21.4 MPa ASTM D 412
Allongement à la rupture 1300 % ASTM D 412
Propriétés diversesValeurUnitéNorme du test
Densité 920 kg/m³ ASTM D 792
Caractéristiques
Transformation
Enduction
Propriétés spéciales
Transparent
Caractéristiques
Copolymère
Résistance Chimique
Résistance à oxydation
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.